    • Indentation across interfaces between stiff and compliant tissues 

      Oyen, ML; Armitage, OE
      Abstract Bone–tendon, bone–ligament and bone–cartilage junctions are multi-tissue interfaces that connect materials that differ by two orders of magnitude in mechanical properties, via gradual variations in mineral content ...
    • Nanoindentation of Hydrated Materials and Tissues 

      Oyen, Michelle L. (Elsevier, 2015-04-04)
      Nanoindentation techniques have recently been adapted for the study of hydrated materials, including biological materials and hydrogels. There are unique challenges associated with handling and testing hydrated samples. For ...
    • Nanoindentation Under Dynamic Conditions 

      Wheeler, Jeffrey M (2009-05-22)
      Nanoindentation has emerged as a leading technique for the investigation of mechanical properties on small volumes of material. Extensive progress has been made in the last 20 years in refining the nstrumentation of ...